MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lucite International Colacryl® DP300 Specialty Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: This is a high molecular weight PMMA resin. PMMA resins are characterised by high physical strength and abrasion resistance.

Applications:
This resin is used in the production of porous polymer molds for the sanitary ware casting industry (pressure casting), and in the production of castings and embedments.

Information provided by Lucite International

Key Words: PMMA; Polymethyl Methacrylate; Polymethylmethacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 80 - 100 µm80 - 100 µm
Viscosity Measurement 6.0 - 8.06.0 - 8.0reduced
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.50 %0.50 %
 
Descriptive Properties
BPO Content (%)0.25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Chemical Sumipex® LG2 Acrylic Resin, High Flow
Lucite International Lucite® 41 Acrylic Bead Resin
Lucite International Lucite® 30B Acrylic Bead Resin
Lucite International Lucite® 6751 Acrylic Bead Resin
Lucite International Lucite® 4G Acrylic Bead Resin

PLUCIT9425 / 150139

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.