MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Americhem Engineered Compounds ColorFast® FRPBT200 PBT, Flame Retarded
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: V-0 rated, unfilled PBT

All information provided by LTL Color Compounders, Inc. LTL was acquired by Americhem in 2014.

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/ccASTM D792
Linear Mold Shrinkage 0.015 - 0.023 cm/cm0.015 - 0.023 in/in0.125 in.; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength at Break 58.6 MPa8500 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 58.6 MPa8500 psi2.0 in/min; ASTM D638
Elongation at Break 80 %80 %2.0 in/min; ASTM D638
Flexural Strength 101 MPa14700 psi2.0 in/min; ASTM D790
Flexural Modulus 2.62 GPa380 ksi2.0 in/min; ASTM D790
Izod Impact, Notched 0.374 J/cm
@Temperature 22.8 °C
0.700 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C160 °FUnannealed (0.250"); ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 - 249 °C450 - 480 °F
Middle Barrel Temperature 238 - 254 °C460 - 490 °F
Front Barrel Temperature 243 - 260 °C470 - 500 °F
Nozzle Temperature 238 - 254 °C460 - 490 °F
Melt Temperature 243 - 260 °C470 - 500 °F
Mold Temperature 48.9 - 76.7 °C120 - 170 °F
Drying Temperature 121 °C250 °F
Dry Time 3 - 4 hour3 - 4 hournominal; maximum drying time of 12 hours
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00127 - 0.00254 cm0.000500 - 0.00100 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLTLC041 / 104426

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.