LE4244R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. This product is only available in certain periods. Applications: LE4244R is intended for insulation of XLPE power cables with rated voltages up to 72 kV. Specifications: IEC 60502.Information provided by Borealis AG |