MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES Plastiblend® ABS HH BK MB
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Availability: North America

Forms: Pellets

Features: High Gloss and High Heat Resistance

Appearance: Black

Processing Method: Injection Molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ASTM D792
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ASTM D785
Tensile Strength 37.2 MPa5400 psiASTM D638
Elongation at Yield 3.1 %3.1 %ASTM D638
Flexural Yield Strength 71.0 MPa10300 psiASTM D790
Flexural Modulus 2.34 GPa340 ksiASTM D790
Izod Impact, Notched  1.12 J/cm
@Thickness 3.17 mm,
Temperature -40.0 °C
2.10 ft-lb/in
@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
 1.49 J/cm
@Thickness 3.17 mm,
Temperature 0.000 °C
2.80 ft-lb/in
@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
 3.04 J/cm
@Thickness 3.17 mm,
Temperature 22.8 °C
5.70 ft-lb/in
@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C201 °FUnannealed; ASTM D648
 106 °C223 °FAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C178 °FUnannealed; ASTM D648
 102 °C216 °FAnnealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES Plastiblend® ABS 8003 A1
Techmer ES Plastiblend® ABS 8003
Ravago Manufacturing Americas Hylac HH34 ABS, Medium Heat Resistance, Medium Impact, DAM
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat
Polykemi AB POLYabs R00 UV4 ABS, High Impact, UV Stabilized

PTPC1157 / 137095

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.