MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman AQ™ 38S Polymer
Categories: Polymer

Material Notes: Product Description: Eastman AQ ™ 38S polymer is a sulfopolyester that disperses directly in hot water without the assistance of amines, cosolvents, surfactants or other additives. AQ 38S polymer aids the dispersion of many hydrophobic ingredients in water-based products and forms clear films at room temperature from aqueous dispersions. Eastman AQ ™polymers differ chiefly in glass transition temperature (Tg) or softening point. As indicated by the number in the product name, Eastman AQ 38S polymer has a Tg of about 38°C. The "S" indicates AQ 38S is supplied as solid pellets. Eastman AQ linear polyesters serve as film formers in numerous cosmetic and personal care applications. Because of its low Tg, Eastman AQ™ 38S forms flexible films on the skin. It imparts a smooth feel to creams, lotions, and sprays and adheres to the skin. Thus, it is useful as a filmformer in sunscreen products, providing excellent water resistance. AQ 38 is added to the water phase and aids the emulsification of oil-phase UV absorbers. AQ 38 provides improved coverage for sprayable sunscreens.

Application/Uses:

  • Caulks and Sealants
  • Creams
  • Lotions
  • Skin care
  • Sprays
  • Sun care
Key Attributes:
  • Aids the emulsification of organic ingredients
  • Low-viscosity hairsprays
  • No neutralization needed
  • Quick drying
  • Water resistant

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.779 g/cc0.0281 lb/in³
Viscosity 970000 cP
@Temperature 200 °C
970000 cP
@Temperature 392 °F
Melt
Viscosity Test 32 - 40 cm³/g0.32 - 0.40 dl/gInherent
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 2.0<= 2.0[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 35.0 - 38.0 °C95.0 - 100 °F
 
Descriptive Properties
AppearancePellets
ColorPale Amber
Hydroxyl Number<10[mg KOH/]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5128 / 222322

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.