Ablebond 862-2 room temperature curing epoxy adhesive is designed for solder pad encapsulation or sealing the head/disk area in floppy disc assemblies. This resilient compound is suitable for bonding materials with mismatched coefficients of thermal expansion. Information provided by Tra-Con Inc. |