MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Petrothene NA247000X01 LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Petrothene NA247000X01 provides a balance of stiffness and tear strength. Typical applications include tamper evident caps and closures. Applications: Caps & Closures

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D1505
Melt Flow 7.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4848ASTM D2240
Tensile Strength, Yield 13.6 MPa1970 psiASTM D638
Elongation at Yield 13 %13 %ASTM D638
Flexural Modulus, 1% Secant 340 MPa49300 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -43.0 °C-45.4 °FASTM D746
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman PE1059 Film Extrusion Polyethylene
Huntsman PE5050 Extrusion Coating Polyethylene
ExxonMobil LDPE LGA 105 Low Density Polyethylene Resin
Westlake EC472 Low Density Polyethylene
Huntsman PE5030 Extrusion Coating Polyethylene

PEQT8855 / 220489

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.