MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Zinc ZA-8 (Zn-8Al-1Cu-0.02Mg), Die Cast
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Recommended Casting Temperature 435-460°C

Key Words: ASTM B791; ASTN B669; UNS Z35635 (Ingot); UNS Z35636 (castings)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 103500 kg load; 10 mm hardened steel ball
Hardness, Knoop 129Estimated from Brinell Value
Hardness, Rockwell A 42Estimated from Brinell Value
Hardness, Rockwell B 65Estimated from Brinell Value
Hardness, Vickers 116Estimated from Brinell Value
Tensile Strength, Ultimate 374 MPa
Tensile Strength, Yield 290 MPa
@Strain 0.2 %
Elongation at Break 8.0 %in 5 cm
Modulus of Elasticity 85.5 GPa
Compressive Strength 252 MPa
Fatigue Strength 103 MPa
@# of Cycles 5.00e+8
Reverse Bend
Fracture Toughness 12.6 MPa-m½
Shear Strength 275 MPa
Charpy Impact, Unnotched 42.0 J
@Thickness 6.35 mm
square bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000620 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 112 J/g
CTE, linear 23.2 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.435 J/g-°C
Thermal Conductivity 115 W/m-K
Melting Point 375 - 404 °C
Solidus 375 °C
Liquidus 404 °C
 
Processing PropertiesOriginal ValueComments
Casting Temperature 435 - 460 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 8.0 - 8.8 %Addition, Casting
 8.2 - 8.8 %Addition, Ingot form
Cadmium, Cd <= 0.0050 %Impurity, Ingot form
 <= 0.0060 %Impurity, Casting
Copper, Cu 0.80 - 1.3 %Addition, Casting
 0.80 - 1.3 %Addition, Ingot form
Iron, Fe <= 0.065 %Impurity, Ingot form
 <= 0.075 %Impurity, Casting
Lead, Pb <= 0.0050 %Impurity, Ingot form
 <= 0.0060 %Impurity, Casting
Magnesium, Mg 0.015 - 0.030 %Addition, Casting
 0.020 - 0.030 %Addition, Ingot form
Tin, Sn <= 0.0020 %Impurity, Ingot form
 <= 0.0030 %Impurity, Casting
Zinc, Zn 89.793 - 90.98 %As balance; Ingot per ASTM B 669
 89.78 - 91.185 %As balance; Castings per ASTM B 791

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zinc ZA-27 (Zn-27Al-2Cu-0.015Mg), Die Cast
Zinc ZA-12 (Zn-11Al-1Cu-0.025Mg), Die Cast
Zinc AG40A (Zinc Alloy 3; Zn-4Al-0.4Mg; Zamak 3), Cast
Zinc AC43A (Zinc Alloy 2; Zn-4Al-2.5Cu-0.04Mg; Number 2 Die Casting Alloy; Zamak 2), Die Cast
304 Stainless Steel

MZN800 / 14566

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.