System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LNP™ THERMOTUF™ Compound V1000UXC Polyamide, Unspecified (Nylon, Unspecified)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
Material Notes:
LNP THERMOTUF V1000UXC compound is based on Super Tough Nylon resin. Added features of this grade include: Impact Modified, UV Stabilized.
Features: Impact Modified,UV Resistant
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.07
g/cc
ASTM D792
Density
1.065
g/cc
ASTM D792
1.08
g/cc
ISO 1183
Moisture Absorption
0.150 - 0.250 %
Injection Molding
0.600 %
23°C/50% RH/24 hrs; ASTM D570
1.00 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.021
-
0.023
cm/cm
24hrs; ASTM D955
0.022
cm/cm
24hrs; ISO 294
Linear Mold Shrinkage, Transverse
0.025
-
0.027
cm/cm
24hrs; ASTM D955
0.026
cm/cm
24hrs; ISO 294
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
39.0
MPa
5 mm/min; ASTM D638
41.0
MPa
5 mm/min; ISO 527
Tensile Strength, Yield
39.0
MPa
5 mm/min; ASTM D638
41.0
MPa
5 mm/min; ISO 527
Elongation at Break
84.5 %
5 mm/min; ASTM D638
165 %
5 mm/min; ISO 527
Elongation at Yield
57.2 %
5 mm/min; ASTM D638
146.7 %
5 mm/min; ISO 527
Tensile Modulus
1650
MPa
1 mm/min; ISO 527
1710
MPa
5 mm/min; ASTM D638
Flexural Strength
53.0
MPa
ISO 178
55.0
MPa
ASTM D790
Flexural Modulus
1700
MPa
ISO 178
2060
MPa
ASTM D790
Izod Impact, Unnotched
NB
ASTM D4812
Izod Impact, Unnotched (ISO)
NB
80*10*4; ISO 180/1U
Dart Drop, Total Energy
49.0
J
ASTM D3763
Impact Test
49.0
J
Multiaxial Impact; ISO 6603
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
134
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
135
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow
133
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
134
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
150
°C
Flatw 80*10*4 sp=64mm; ISO 75/Bf
192
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
147
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
193
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Processing Properties
Original Value
Comments
Zone 2
270
-
280
°C
Zone 3
290
-
300
°C
Melt Temperature
270
-
295
°C
Injection Molding
Mold Temperature
50.0
-
95.0
°C
Drying Temperature
80.0
°C
Injection Molding
Dry Time
4.00
hour
Injection Molding
Back Pressure
0.300
-
0.700
MPa
Screw Speed
10
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH82021 / 289968
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.