MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Wacker Powersil® 3540 MH Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product description: POWERSIL® 3540 MH silicone rubber is a one component, ready to use, addition-curing compound that cures to an electrical insulating, highly erosion resistive silicone elastomer. POWERSIL® 3540 MH shows fast curing in comparison to conventional silicone rubber. Curing time is reduced by (30 … 50) % depending on the wall thickness and on the available machinery and runner system. No peroxide decomposition products are released while curing.

Special features:

  • easy demolding
  • excellent dielectric properties
  • high arcing and tracking resistance
  • no unpleasant smell caused by peroxides
  • no inhibition by oxygen
Application: POWERSIL® 3540 MH is especially designed for T&D applications. Because of its excellent mechanical properties POWERSIL® 3540 MH is prone for use in “cable accessories” applications. Especially thick walled articles can take advantage of the fast curing material.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3838ISO 868
Tensile Strength at Break 10.0 MPa1450 psiISO 37
Elongation at Break 900 %900 %ISO 37
Tear Strength 28.0 kN/m160 pliASTM 624 B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.8
@Frequency 50 Hz
2.8
@Frequency 50 Hz
IEC 60250
Dielectric Strength >= 23.0 kV/mm>= 584 kV/inIEC 60243
Dissipation Factor 0.00030
@Frequency 50 Hz
0.00030
@Frequency 50 Hz
IEC 60250
Arc Resistance >= 240 sec>= 240 secIEC 61621
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Treatment Temp. 165 °C
0.250 hour
@Treatment Temp. 329 °F
post-cured 4hr at 150°C
 
Descriptive Properties
Colorwhite
Track Resistance>1A 3.5IEC 60587

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Trelleborg S650 Silicone Rubber
Rogers Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate
Applied Silicone 40072 Liquid Silicone Rubber, 25-10:1, Implant Grade

PWACK9388 / 204917

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.