MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chi Mei Kibilac® PW-997S ASA Polymer
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: Extrusion

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccISO1183
Melt Flow 3.8 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Melt Volume Rate (ml/10 min); ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 88.0 MPaH358/30; ISO 2039-1
Tensile Strength at Break 42.0 MPa50 mm/min; ISO 179/2D
Tensile Strength, Yield 48.0 MPa50 mm/min; ISO 527
Elongation at Break 80 %50 mm/min; ISO 527
Flexural Strength 65.0 MPa2 mm/min; ISO 178
Flexural Modulus 1.80 GPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) NBISO 180/1C
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 2.05 J/cm²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °Cunannealed; ISO 75
 96.0 °Cannealed; ISO 75
Vicat Softening Point 92.0 °C
@Load 5.00 kg
50°C/hr; ISO 306
 95.0 °C
@Load 5.00 kg
120°C/hr; ISO 306
 105 °C
@Load 1.00 kg
50°C/hr; ISO 306
 108 °C
@Load 1.00 kg
120°C/hr; ISO 306
Flammability, UL94 HBUL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Kibilac® PW-978B ASA, High Heat
Chi Mei Kibilac® PW-957 ASA Polymer
INEOS Styrolution Luran® S 797S White 35962 ASA
A. Schulman Diamond ASA S140
Chi Mei Wonderlite® PC-110U Polycarbonate - UV Stabilized

PCHI988 / 109476

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.