MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Wollite 45 Insulating Castable
Categories: Ceramic

Material Notes: Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting complex shapes and parts.

Applications

  • Secondary insulation
  • Foam blocks
  • Floats
  • Spouts

Advantages

  • Non-wetting
  • Does not require preheating prior to usage
  • Low K-factor
  • Thermal shock resistant
  • Ceramic fiber free
  • Non-asbestos

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.721 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00174 GPa
@Temperature 375 °C
Compressive Strength 5.86 MPa
@Temperature 375 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.120 W/m-K
 0.140 W/m-K
@Temperature 250 °C
 0.180 W/m-K
@Temperature 600 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek O'-Sialon Non-Oxide Ceramic
Pyrotek F-51 Dense Machinable Board
Pyrotek Valcor® G Pre-Cast Shapes
Pyrotek Valcor® G-AZ Pre-Cast Shapes
Pyrotek Wollite 30 Insulating Castable

CPYRO164 / 1882

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.