MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Fire-refined Tough Pitch Copper, UNS C12500, H06 Temper, Flat
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Extra Hard

Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Brazing, Butt Weld; Fair Suitability – Gas Shielded Arc Welding

Common Fabrication Processes: Blanking, Coining, Coppersmithing, Drawing, Etching, Forming and Bending, Heading and Upsetting, Hot Forging and Pressing, Piercing and Punching, Roll Threading and Knurling, Shearing, Spinning, Squeezing and Swaging, Stamping

Typical uses: Building Fronts; Downspouts; Flashing; Gutters; Roofing; Screening; Spouting; Gaskets; Radiators; Bus Bars; Commutator Segments; Contacts; Radio Parts; Switches; Terminals; Anodes; Chemical Process Equipment; Kettles; Pans; Printing Rolls; Road Bed Expansion Plates; Rotating Bands; Vats

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.323 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 55.0 ksi
@Thickness 0.0762 mm
 55.0 ksi
@Thickness 0.508 mm
Tensile Strength, Yield 53.0 ksi
@Thickness 0.0762 mm
0.2% Offset
 53.0 ksi
@Thickness 0.508 mm
0.2% Offset
Elongation at Break 1.0 %
@Thickness 0.0762 mm
 2.0 %
@Thickness 0.508 mm
Tensile Modulus 17400 ksi
Modulus of Rigidity 6400 ksi
Poissons Ratio 0.36Calculated
Machinability 20 %
Forgeability 65 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000187 ohm-cm92% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.30 µin/in-°F
@Temperature 20.0 - 100 °C
 9.60 µin/in-°F
@Temperature 20.0 - 200 °C
 9.80 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0920 BTU/lb-°F
Thermal Conductivity 202 BTU-in/hr-ft²-°F
Melting Point 1949 - 1981 °F
Solidus 1949 °F
Liquidus 1981 °F
Annealing Point 750 - 1200 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1400 - 1600 °F
 
Component Elements PropertiesOriginal ValueComments
Antimony, Sb <= 0.0030 %
Arsenic, As <= 0.012 %
Bismuth, Bi <= 0.0030 %
Copper, Cu >= 99.88 %
Nickel, Ni <= 0.050 %
Tellurium, Te <= 0.025 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC12500x3 / 292755

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.