MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips K-Resin® XK41 Styrene-Butadiene Copolymer, Sheet Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrene-Butadiene Copolymer

Customer Benefits: XK41 is an extrusion grade of K-Resin SB copolymer designed specifically for improved performance in blends with general purpose polystyrene. It is easily processed by extrusion and gives thermoformed parts with excellent detail on fast production cycles. Compared to KR05, XK41 offers greater polystyrene acceptance with equivalent processability. Thermoformed parts have very good clarity, very good toughness, and good stiffness.

Applications: Major applications include thermoformed blister packs, cups and lids, and portion packages.

Processing Recommendations:
Melt Temperature: 218°C maximum. High shear and restrictive type screws tend to degrade the melt. Generally no need to dry resin.

Specification Data: When combined with at least 8% food grade polystyrene to produce articles for food contact, XK41 complies with FDA Regulation 21 CFR 177.1640.

Data provided by Chevron Phillips Chemical Company LP.

Ineos Styrolution acquired the K-Resin® product line from Chevron Phillips Chemical Company in 2016. This grade was previously discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccASTM D792
Melt Flow 7.5 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61ASTM D2240
Tensile Strength, Yield 18.8 MPa2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Elongation at Break 251 %2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Flexural Yield Strength 29.5 MPaTest specimens were injection molded by ASTM D1897; ASTM D790
Flexural Modulus 1.2075 GPaTest specimens were injection molded by ASTM D1897; ASTM D790
Izod Impact, Notched 0.430 J/cmASTM D256
Instrumented Impact Total Energy 28.2 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °CASTM D648
Vicat Softening Point 69.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 89.3 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 218 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips K-Resin® XK40 Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade
Chevron Phillips K-Resin® DK13 Styrene-Butadiene Copolymer, Film Grade

PCHEVK85 / 20290

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.