Description: Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. It can be used for medical device applications as it meets USP Class VI testing and ISO 10993-5 for cytotoxicity. MasterSil 153Med is an addition cured system and does not require exposure to air for cross-linking. It has a convenient one to one mix ratio by weight, and will not outgas while curing. It is 100% solids and contains no solvents. MasterSil 153Med exhibits typical silicone flexibility and high temperature resistance. MasterSil 153Med has a long working life and very low exotherm. It bonds well to a wide variety of substrates including most metals, many plastics, glass and ceramic. Most importantly, it will bond well to cured silicone rubber. It has good electrical insulation properties. Its flexibility allows it to withstand severe thermal cycling and resist vibration and shock. It has a self priming feature that enhances the bonding properties of the system. Also, it is very water resistant. MasterSil 153Med is translucent and is serviceable over the broad temperature range of -65°F to +400°F. It is widely used in medical device applications where high flexibility and splendid temperature resistance are required. Product Advantages: - Addition cured; no by-products released during cure; does not require air for curing.
- Low exotherm; very long pot life. Very low shrinkage upon cure.
- Readily cures at ambient temperatures or faster cure at elevated temperatures.
- Softer durometer; offers repairability.
- Bonds well to a variety of substrates including silicone rubber. Self priming feature.
- Good electrical insulation properties; highly resistant to water.
- Outstanding flexibility combined with high temperature resistance.
- Meets USP Class VI and ISO 10993-5 specifications.
Key Features - Passes USP Class VI testing
- Addition cured system
- Self priming feature
- Meets ISO 10993-5 specifications
- Serviceable from -65°F to +400°F
- Paste consistency
Information provided by MasterBond® |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |