MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mi-Tech Metals HD17 Tungsten-Based Metal
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.

Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduces soldering or erosion problems. To increase the machinability of this brittle metal, alloying elements are added and practical use of tungsten is possible for die casting tools.

Used in resistance brazing and high temp applications. Used as counter weights and counter balances, radiation shielding components, tool shanks for boring bars and other tools for chatter-free machining.

Data provided by Mi-Tech Metals.

Key Words: Class 1 Tungsten Alloys; AMS 7725B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 17.0 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 32
Tensile Strength, Ultimate 758 MPa
Tensile Strength, Yield 550 MPa
@Strain 0.2 %
Elongation at Break 6.0 %in 50 mm
Modulus of Elasticity 276 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000120 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.40 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 96.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 4.0 %
Nickel, Ni 6.0 %
Tungsten, W 90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mi-Tech Metals HD17BB Tungsten-Based Metal
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3)
Nitronic 40 Stainless Steel Plate
Mi-Tech Metals Super Chatter Free™ HD17.7 Tungsten-Based Metal
Plansee Ta2.5W Tantalum-Tungsten 2.5 Alloy

NMITECH24 / 18434

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.