MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions CPVC MC500 Polyvinyl Chloride, Chlorinated (CPVC)
Categories: Polymer; Thermoplastic; Vinyl (PVC); Chlorinated PVC (CPVC)

Material Notes: The Geon MC500 CPVC is an injection molding fittings compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. Geon MC500 demonstrates superior processability and excellent thermal stability.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D785
Tensile Strength, Yield 55.2 MPa
@Temperature 23.0 °C
ASTM D638
Tensile Modulus 2990 MPa
@Temperature 23.0 °C
ASTM D638
Flexural Yield Strength 103 MPaASTM D790
Flexural Modulus 3380 MPaASTM D790
Izod Impact, Notched 96.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °CAnnealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 198 - 210 °C
 
Descriptive Properties
FormsPellets
Generic MaterialCPVC
Generic NamePolyvinyl Chloride, Chlorinated (CPVC)
Processing MethodInjection Molding
PVC Cell Classification23447ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesFittings
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions CPVC EC950 Polyvinyl Chloride, Chlorinated (CPVC)
Geon® Performance Solutions CPVC MC250 Polyvinyl Chloride, Chlorinated (CPVC)
Arkema Lucalor® PEY 221 CPVC, Pipe Grade
Geon® Performance Solutions CPVC EC900 Polyvinyl Chloride, Chlorinated (CPVC)
Geon® Performance Solutions CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC)

PH0POL1128 / 145697

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.