MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Elkem LC FeSi 65 Low Carbon Ferrosilicon
Categories: Metal

Material Notes: This product is added as a deoxidant and as an alloying element to steels that require a special low carbon content, e.g. non-grain oriented electrical steels. Low Carbon FeSi 65 lowers the electrical conductivity and magnetostriction of electrical steels. When FeSi 75% dissolves in steel, it increases the temperature of the bath while FeSi 65% is almost temperature neutral,

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.90 g/cc0.0686 lb/in³
Density 3.50 g/cc0.126 lb/in³
Solubility in Water 0.00 %0.00 %Insoluble
Particle Size 3000 - 50000 µm3000 - 50000 µm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 1037 J/g446.1 BTU/lb
Specific Heat Capacity 0.776 J/g-°C0.185 BTU/lb-°F
Melting Point 1208 - 1300 °C2206 - 2370 °F
Solidus 1208 °C2206 °F
Liquidus 1300 °C2370 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.50 %<= 0.50 %
Carbon, C <= 0.020 %<= 0.020 %
Iron, Fe >= 33.34 %>= 33.34 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si 64 - 66 %64 - 66 %
Titanium, Ti <= 0.12 %<= 0.12 %
 
Descriptive Properties
Angle of Repose40°-60°
Solubility in alkalisOxidizes with formation of H2 in Alkalis
Solubility in Hydrofluoric AcidSoluble with formation of SiF4
Solubility in Mineral AcidsSoluble with formation of H2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
316 Stainless Steel, annealed sheet
AK Steel 316 Austenitic Stainless steel
303 Stainless Steel, annealed
Hardwire 3SX-21.5-12 High Density Composite

NELKEM20 / 16178

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.