MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical PE1311 PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: General Description: PE1311, homopolymer made by emulsion polymerization, is a high-viscosity PVC resin with pseudo-plastic flow property PE1311 has an good chemical foaming with low density and fine cell.

Main Applications: Dipping, Low density foam layer in wall coverings and flooring, Synthetic leather Automotive underbody coater, High foaming products

CAS No: 9002-86-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.406 g/cc
Bulk Density 0.310 - 0.410 g/ccASTM D1895
Volatiles <= 0.30 %
@Temperature 110 °C,
Time 3600 sec
ASTM D3030-90
Brookfield Viscosity 10000 - 60000 cPDOP 60phr, 6RPM; ASTM D1824
Viscosity Measurement >= 5.0
@Pressure 0.400 MPa
[g/sec], DOP 60phr, Severs; ASTM D1823
Molecular Weight 60000 - 150000 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 302 °C
Ignition Temperature 435 °CAutoignition
 
Descriptive Properties
Degree of Polymerization1200-130030°C, JIS K 6720-2
K-Value70DIN53726 / ISO1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 1131-57D Wire & Cable Flexible PVC
AlphaGary Garaflex™ 131 T Vinyl Thermoplastic Elastomer
Arkema Lacovyl® PE 1311 H PVC
AISI Type 316L Stainless Steel, annealed sheet
AISI 8640 Steel, quenched 845°C (1550°F), 650°C (1200°F) temper

PLAY721 / 148731

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.