System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Sciengy PEEK-SGRN10FP PEEK
Categories:
Polymer
;
Thermoplastic
;
Polyketone
;
Polyetheretherketone (PEEK)
;
Polyetheretherketone, PEEK, Unreinforced
Material Notes:
PEEK-SGRN10FP is a fine powder type. It is applied to injection, mold pressing, extrusion and modification.
Information provided by Shandong Sciengy New Materials Co. Ltd
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Bulk Density
>=
0.380
g/cc
ISO 1183
Density
1.30
g/cc
ISO 1183
Particle Size
90
µm
D50; ISO 13320-1
Melt Flow
13
g/10 min
@Load 5.00 kg,
Temperature 380 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength
98.0
MPa
ISO 527
Elongation at Break
45 %
ISO 527
Tensile Modulus
3700
MPa
ISO 527
Flexural Strength
162
MPa
ISO 178
Flexural Modulus
4.00
GPa
ISO 178
Charpy Impact, Notched
11.0
kJ/m²
IS0 179
Thermal Properties
Original Value
Comments
Melting Point
343
°C
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi)
152
°C
ISO 75
Glass Transition Temp, Tg
143
°C
ISO 11357
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSCIE070 / 297117
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.