Georgia Gulf ProTherm® 4353 is a CPVC powder blend designed for extrusion of large diameter, heavy wall industrial pipe requiring high temperature and good chemical resistance. Processing and stability along with overall physical properties are excellent. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |