MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shin-Etsu Silicones KE-5006U PVMQ Silicone
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: ShinEtsu KE5006 U is a phenyl (PVMQ) silicone product. This product is designed for good low temperature characteristics.

Product Features:

  • A broad range of service temperatures from 100 to +260°C (148 to +500°F.)
Typical Applications:
  • Low temperature gaskets.
  • Low temperature packing..

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55
Tensile Strength at Break 1600 psi
Elongation at Break 500 %
Tear Strength 185 pliDie B
Compression Set 33 %
@Temperature 150 °C,
Time 252000 sec
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -100 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 150 °C
Post
 
Descriptive Properties
Cure AgentDCBP
Cure TypePost Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shin-Etsu Silicones KE-571U Silicone Elastomer
Shin-Etsu Silicones KE-581U Silicone Elastomer
Shin-Etsu Silicones KE-971TU Silicone Elastomer
Precision Polymer Engineering S40H Silicone Rubber
Shin-Etsu Silicones KE-1843 Silicone, RTV Adhesive/Sealant

PSHIN221 / 177732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.