MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound OCL36 Polyphenylene Sulfide, Linear (PPS, Linear) (Americas)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LNP LUBRICOMP OCL36 compound is based on Polyphenylene Sulfide (PPS) - linear resin containing 30% carbon fiber and 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.

Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Wear resistant,Electrically Conductive,Structural

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccASTM D792
 1.52 g/ccISO 1183
Moisture Absorption 0.0300 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm24hrs; ASTM D955
 0.0020 - 0.0040 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0030 - 0.0040 cm/cm24hrs; ASTM D955
 0.0036 - 0.0040 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 166 MPaISO 527
 168 MPaASTM D638
Elongation at Break 1.1 %ISO 527
 1.4 %ASTM D638
Tensile Modulus 21510 MPa5 mm/min; ASTM D638
 30680 MPa1 mm/min; ISO 527
Flexural Strength 259 MPaASTM D790
 262 MPaISO 178
Flexural Modulus 21110 MPaASTM D790
 21200 MPaISO 178
Izod Impact Notched 58.0 JASTM D256
Izod Impact, Unnotched 443 J/mASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 31.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 15.0 Jpeak; ASTM D3763
Impact Test 2.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.39ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.34ASTM D3702 Modified: Manual
K (wear) Factor 19.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 16.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 17.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 34.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 34.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 263 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 267 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.80 mm
UL 94 by SABIC-IP
 
Processing PropertiesOriginal ValueComments
Zone 2 320 - 330 °C
Zone 3 330 - 345 °C
Melt Temperature 315 - 320 °CInjection Molding
Mold Temperature 140 - 165 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80910 / 288857

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.