MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Schmolz + Bickenbach MoldMAX® SC Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Description: Brush Wellman’s MoldMAX® SC is a high conductivity copper mold alloy with good strength. MoldMAX® SC is used as blow mold cavities, injection mold cores and cavities and hot runners. The alloy provides excellent toughness, and the highest conductivity of any alloy with tensile strength in excess of 100,000 psi.

Information provided by Schmolz + Bickenbach

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 2020
Tensile Strength, Ultimate 724 MPa105000 psi
Tensile Strength, Yield 621 MPa
@Strain 0.2 %
90000 psi
@Strain 0.2 %
Elongation at Yield 15 %15 %
Modulus of Elasticity 138 GPa20000 ksi
Fatigue Strength >= 240 MPa
@# of Cycles 1.00e+7
>= 34800 psi
@# of Cycles 1.00e+7
(R=-1)
Impact Test 54.2 J40.0 ft-lb
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C9.80 µin/in-°F
Specific Heat Capacity 0.414 J/g-°C
@Temperature 100 °C
0.0990 BTU/lb-°F
@Temperature 212 °F
Thermal Conductivity 20.9 W/m-K
@Temperature 100 °C
145 BTU-in/hr-ft²-°F
@Temperature 212 °F
Melting Point >= 1040 °C>= 1900 °Fapproximate
Solidus 1040 °C1900 °Fapproximate
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.20 - 0.60 %0.20 - 0.60 %
Copper, Cu 97.2 - 98.4 %97.2 - 98.4 %
Nickel, Ni 1.4 - 2.2 %1.4 - 2.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schmolz + Bickenbach MoldMAX LH® Low Hard - Copper Alloy
Cadi MOLD-MOR™ 3
Brush Wellman Beryllium Copper Alloy 165 Strip; 1/2H (TD02) Temper (UNS C17000)
Brush Wellman Beryllium Copper Alloy 10 Strip; HTC Temper (UNS C17500)
Bohler-Uddeholm BeCu Alloy 172 Mold Material

NSCHMO030 / 125903

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.