Mix Ratio with GY 6010 is 5. Comments/Applications: Reduces gel time and cure schedule for adhesives and other fast cure epoxy systems. Benzyl dimethyl amine (BDMA)-tertiary amine accelerator. Compatible with anhydride and polyamide hardeners. Flexible mix ratio = 0.5 - 10.0 PHR, with GY 6010. Data provided by Ciba Specialty Chemicals. Ciba Specialty Chemicals has been acquired by Huntsman. |