MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lucite International Colacryl® TS2027 Acrylic Dental Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.

Information provided by Lucite International

Key Words: Methyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 60 - 76 µm
Molecular Weight 300000 - 900000 g/mol
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 min
@Pressure 0.207 MPa,
Temperature 40.0 °C
 
Descriptive Properties
Pour Time (min)2 - 3
Residual peroxide (%)0.9 - 1.3
Set Time (min)14 - 20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lucite International Colacryl® D120 Acrylic Dental Resin
Lucite International Colacryl® D80FC Acrylic Dental Resin
Lucite International Colacryl® TS2082 Acrylic Resin
Lucite International Colacryl® TS 1672 Acrylic Orthodontic Polymer
Lucite International Colacryl® TS 1649 Acrylic Orthodontic Polymer

PLUCIT9445 / 150159

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.