MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Aremco’s refractory coatings offer the ultimate protection of high temperature components used in the processing of ceramics, glass, metals, and plastics.

Features

  • Ultra Hi-Temp Resistance
  • Non-Wetted by Molten Metals, Salts, Glass & Plastics
  • High Lubricity for Easy Part Release
  • Minimizes Cast Surface Defects
  • Increases Mold & Die Life
  • For Use in Oxidizing, Reducing & Vacuum Atmospheres
Applications:
  • Composite Forming
  • Glass Forming
  • Metal Casting
  • Injection Molding
  • Ceramic Hot-Pressing
  • Metal Powder Sintering
  • Welding
  • Brazing
Product Highlights: This phosphate-bonded, single-part alumina coating bonds exceptionally well to dense refractories, providing high abrasion and corrosion resistance for operating temperatures to 3200°F (1760°C).

Key Words: Coatings
Vendors: Aremco’s Pyro-Paint refractory coatings offer the ultimate protection of high temperature graphite, metal and refractory structures used in the processing of ceramics, glasses, metals, and plastics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.38 g/cc2.38 g/cc
Solids Content 53.7 %53.7 %by volume
 76 %76 %by weight
pH 2.0 - 3.02.0 - 3.0Coating pH
Viscosity 5000 - 7000 cP5000 - 7000 cP
Thickness 25.4 microns1.00 milDry Film Thickness
 48.3 microns1.90 milWet Film Thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1760 °C3200 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 50.0 - 90.0 °C122 - 194 °FApplication Temp
Cure Time 120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
after 1 hr air drying, 1 hr at 800°F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorWhite
Dry Film Coverage ft2/gal861at 1 mil
Thinner634AL-T
Weight/Gallon16.5 lbs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Zirconia ZR-RIG Zirconia Rigidizer
Anderman Ceramics EZZ 66P Zircon
Anderman Ceramics EZM 96 Zirconia, 96.5%, Magnesia-Stabilized
Aremco Ceramacast™ 646 Castable Ceramic
MarkeTech Repton 868 Zirconia + 8 mol% Yttria (YSZ)

CAREM58A / 138323

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.