MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo INSPIRE™ TF1302 Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: INSPIRE TF7000 ES Natural Performance Polymer DA™ is a very high stiffness (2400 MPa) TPO designed for instrument panel upper and lower components, as well as other interior trim applications where stiffness, good impact resistance, and good molded-in-color part aesthetics are important. Its high melt flow rate also allows for rapid filling of large parts in the injection molding process.

Main Characteristics:

  • Excellent Surface Aesthetics
  • Good Scratch & Mar Resistance
  • Instrument Panel Uppers/Lowers
  • Interior Trim Applications
  • High Flow
  • Approved on DaimlerChrylser MS-DC265D
Automotive Specifications:
  • CHRYSLER MS-DC-265 Type D
  • IMDS ID 30867190 Color: Charcoal
  • GM QK 004023 U Color: Charcoal

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccASTM D792B
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPaASTM D638
Elongation at Yield 6.0 %ASTM D638
Flexural Modulus 1210 MPaASTM D790A
Izod Impact, Notched (ISO) NBASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °CUnannealed; ISO 75-2/B
 93.3 °CUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo INSPIRE™ TF 1301 Thermoplastic Polyolefin
ExxonMobil PP8114E1 Impact Copolymer
Dow AFFINITY™ EG 8185 Polyolefin Plastomer (POP)
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP)

PDOW1150C / 30366

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.