MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exxtra™ Soft EMA5024 ExCo Ethylene Methyl Acrylate, Extrusion Coating Grade
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Coating Grade

Material Notes: Exxtra™ Soft EMA5024 is an ethylene methyl acrylate copolymer that can be used for making alloys, blends and compounds. It can also be injection molded where softness and flexibility are required. It is an excellent grade for coextrusion coating and extrusion lamination where good interlayer adhesion between poylethylene, polypropylene, nylon, PVdC, or other substrates is required.

Availability: Latin America, North America

Additive: Antiblock: No; Slip: No; Thermal Stabilizer: Yes

Applications: Coextrusion Coating; Demanding Heat Seals; Extrusion Coating; Extrusion Lamination; Food Packaging; Industrial Packaging; Low Neck In, Low Line Speed Coatings; Masterbatch Base Resin; Thermal Lamination

Information provided by ExxonMobil.

Key Words: Optema™ TC 221 ExCo
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.944 g/ccASTM D1505
Methyl Acrylate Content 24 %ExxonMobil Method
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Neck In 4.20 in
@Temperature 295 °C
656 ft/min, constant output @ 35 rpm; ExxonMobil Method
 5.50 in
@Temperature 295 °C
328 ft/min, constant output @ 35 rpm; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 164 °FPeak; ExxonMobil Method
Vicat Softening Point 114 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEX98902 / 238284

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.