MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NYC YT3WBHQ Y2O3 Powder for Spray Coating
Categories: Ceramic; Oxide

Material Notes: High purity granules produced in clean environment. Uses include semiconductor / LCD industries and electroceramics.
  • Narrow particle size distribution
  • Tailorable for each spray coating technology
  • No clogging in high efficiency spray coating

Key Words: Y2O3, Yttria, Yttrium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.40 - 1.60 g/cc0.0506 - 0.0578 lb/in³JIS K5101
Loss On Ignition <= 0.50 %
@Temperature 1000 °C,
Time 3600 sec
<= 0.50 %
@Temperature 1830 °F,
Time 1.00 hour
Particle Size 30 - 40 µm30 - 40 µmAverage; for outer type spray system; Microtrac HRA
 40 - 50 µm40 - 50 µmAverage; for inner type spray system; Microtrac HRA
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 <= 0.0020 %<= 0.0020 %ICP-AES
Na2O <= 0.0010 %<= 0.0010 %AA
Y2O3 >= 99.99 %>= 99.99 %TREO
 
Descriptive Properties
Angle of Repose24 - 26°JIS K5101

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
H.C. Starck Amperit® 847.6 Agglomerated Yttria (Y2O3)
Yttrium Oxide, Y2O3
H.C. Starck Amperit® 849.054 Sintered Yttria (Y2O3)
NYC YT3X Y2O3 Powder
NYC YT3CP Y2O3 Powder

CNYC991 / 125939

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.