MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ganpati Exim Rubber Processing Oil
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Rubber Processing Oil has predominant number of saturated hydrocarbons. It has low solvency powder (the high aniline point), excellent resistance to oxidation & color stability by heat & ultraviolet.
Applications: RUBBER PROCESSING OIL is suitable for different types of rubber (both natural & synthetic) requiring good low-temperature flexibility, non-staining, color stability and low heat-buildup properties.
Benefits: Improves the process ability of rubber during mixing, milling & extruding by reducing its viscosity, yet retaining the desirable physical properties of the high molecular weight polymer.
Presence of oil also permits the incorporation of dry compounding ingredients into finished rubber articles. Modify the physical properties of the vulcanizate.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Kinematic Viscosity at 100°C (212°F) 28 - 54 cSt28 - 54 cSt
Ash 0.080 %0.080 %
 
Thermal PropertiesMetricEnglishComments
Pour Point 23.0 - 53.0 °C73.4 - 127 °F
Flash Point 225 - 254 °C437 - 489 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.020 %0.020 %
 
Descriptive Properties
Color>8
Content0.0022Asphalthenes
 0.046T. sulphur
 0.16 ppmPotassium
 0.468 ppmSodium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI085 / 317369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.