MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Alpase M-5™ Aluminum Mold Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:
  • Excellent weldability
  • Surface Condition - Machined top and bottom to reduce costly handling and machining steps
  • Dimensional Stability - High dimensional stability during and after machining
  • Polishing - Good polishing properties
  • Good Anodizing and Hard Coating properties
  • Corrosion Resistance - Excellent corrosion resistance in many applications
  • Low density offers a 5% weight savings over other cast products
  • Very consistent hardness and mechanical properties throughout its entire thickness range, regardless of size.
  • Vacuum tight microstructure

Applications: Injection Molds, Blow Molds, Structural Foam Molds, and Rubber Molds. Additional uses include: Vacuum Forming Tools, Compression Molds, Heating and Cooling Plates and proven Semi-conductor Transfer Chamber applications.

Sizes: Thickness up to 30 inches; Width up to 88 inches; Length up to 195 inches.

Typical data provided by Alpase.

Key Words: Aluminium; U/T inspected to MIL-Spec 2154 Class A
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.66 g/cc0.0960 lb/in³
 2.80 g/cc0.101 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 7070
Tensile Strength, Ultimate 283 MPa41000 psi
Tensile Strength, Yield 124 MPa18000 psi
Modulus of Elasticity 71.0 GPa10300 ksi
 74.5 GPa10800 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000590 ohm-cm0.0000590 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  23.2 µm/m-°C
@Temperature 20.0 - 100 °C
12.9 µin/in-°F
@Temperature 68.0 - 212 °F
 23.8 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 139 W/m-K962 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alpase M-1™ Aluminum Mold Plate
Alcoa MIC-6 Aluminum Mold Alloy
Alclad Aluminum 6061-T6, T651
Aluminum 6061-T6; 6061-T651
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding

NALPASE4 / 131319

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.