MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reynolds Brush-On® 50 Brushable Polyurethane Rubber Compounds
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: Smooth-On’s Brush-On™ Series of mold rubbers are extremely versatile and are famous for their abrasion resistance and high tear strength. They have the convenience of a one-to-one mix ratio and are easy to mix and apply with a brush or spatula. Brush-On™ 35, 40, 50 & 60 paint onto vertical surfaces without sagging and will cure with negligible shrinkage to durable rubbers that perform and last in production. Each will capture exact detail from any original model. Brush-On™ 35 is the softest of the series and offers the most flexibility and is used for models with deep undercuts. Brush-On™ 35 & 40 can be inverted and used to make glove molds. Brush-On™ 50 and Brush-On™ 60 possess superior abrasion resistance and tear strength and are ideal for casting concrete and hard plasters in applications where less flexibility is required. These products are compatible. For example, you can apply two coats of Brush-On™ 40 and back it up with two coats of Brush-On™ 50 or 60. All three rubbers are suitable for reproducing sculpture, architectural restoration and production casting of concrete.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D-1475
Linear Mold Shrinkage <= 0.0010 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50ASTM D-2240
Tensile Strength 500 psiASTM D-412
Elongation at Break 400 %ASTM D-412
Tear Strength 80.0 pliDie C; ASTM D-624
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 hourOvernight
Pot Life 20.0 minASTM D-2471
 
Descriptive Properties
ColorOff-White
Mix Ratio100A:125Bby weight
 1A:1Bby volume
Mixed ViscosityBrushable
Specific Volume23.7[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN084 / 296785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.