MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chengdu Letain LTP8275 PPS Composite Material
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LTP 8200 serials is reinforced composite materials with high performance based on PPS, and are extensively applied in injection mold to structure and parts of electric appliance and automobiles. It is used to replace materials of ABS, AES, AS, ASA, PC/ABS serial. The LTP 8200 serials materials have the characteristics of high impact strength, high dimensional stability, high flow power and low moisture absorption.

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ASTM-D792
Water Absorption 0.10 %0.10 %ASTM-D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in80×80×3.0
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in80×80×3.0
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 80.0 MPa11600 psiGB1040
Elongation at Break 12 %12 %GB/T1040
Flexural Strength 120 MPa17400 psiGB/T1042
Izod Impact, Notched (ISO) 128 kJ/m²60.9 ft-lb/in²GB/T1043
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+13 ohm-cm3.00e+13 ohm-cmGB/T1410
Dielectric Constant 3.5
@Frequency 1000 Hz
3.5
@Frequency 1000 Hz
GB/T1409
Dielectric Strength 15.0 kV/mm381 kV/inASTM-D149
Dielectric Loss Index 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
GB/T1409
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 110 °C230 °FGB1634
Flammability, UL94 HBHB
 
Descriptive Properties
Arc index500000000000000[V], UL746A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGLT009 / 255862

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.