MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond F211 General Purpose Fiber Optic Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND F211 is a general purpose fiber optic epoxy adhesive recommended for bonding and small volume potting applications where superior wetting and physical properties are needed at both high and low temperatures. This two component adhesive contains no solvents, has a long pot life at room temperature and develops strong, tough bonds (after a short cure at high temperatures) for a wide range of materials that includes glass fibers, ceramics, most metals and many plastics, Fully cured TRA-BOND F211 develops a dark amber color which provides a ready visual indication of wicking. It has excellent impact and thermal shock resistance, low permeability to gases and vapors, and is resistant to wet or dry autoclave cycles. An additional post-cure of 30 minutes at 150°C is recommended when application temperatures higher than 150°C are anticipated.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccMixed
Viscosity 9800 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88
Izod Impact, Notched 0.500 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.50e+15 ohm-cm
Dielectric Constant 4.2
@Frequency 1000 Hz
Dielectric Strength 375 V/mil
Dissipation Factor 0.020
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 175 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 150 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 125 °C
 3.00 hour
@Temperature 100 °C
 30.0 min
@Temperature 150 °C
Pot Life 300 min
 
Descriptive Properties
Color Amber
Heat Distortion Temperature °C148
Mix Ratio, parts by weight100/20Resin/Hardener
Outgassing, NASA Passes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A-Glass Fiber, Generic

PTRAC248 / 71176

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.