MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Terraloy™ BP 13000A Thermoplastic Starch + PP
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Notes: Terraloy™ BP-13000A is a Thermoplastic Starch/PP ready-to-process compound that contains up to 30% of TPS renewable content. This compound is intended for injection molding as well as extrusion applications.

Processing Method: Extrusion; Injection Molding

Forms: Pellets

Additional Information: Biobased Content: < 30.0

Information Provided by Teknor Apex

Key Words: TPS, PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.997 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3040 psiASTM D638
Elongation at Break 75 %ASTM D638
Tensile Modulus 163000 psiASTM D638
Flexural Strength 4720 psi
@Strain 5.0 %
ASTM D790B
Flexural Modulus, 1% Secant 154000 psiASTM D790B
Izod Impact, Notched 1.20 ft-lb/inASTM D256
Izod Impact, Unnotched 22.0 ft-lb/inASTM D4812

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unitika TERRAMAC TE-7000 Polylactic Acid (PLA)
BiologiQ EcoStarch GS270 Thermoplastic Starch
Teknor Apex Terraloy™ MB 13000A Thermoplastic Starch + PP
RTP Company RTP 2099 X 121249 A Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 88% Renewable Resource Content
RTP Company RTP 2099 X 124790 C Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Standard Nucleator - 78% Renewable Resource Content

PTEKNO807 / 128988

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.