MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Johnson Matthey Orobraze™ 990 Gold Brazing Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Solder/Braze Alloy

Material Notes: Orobraze 990 is manufactured to the highest quality to meet the needs of the aerospace, thermionic component, nuclear and chemical industries. Its properties and uses are similar to those of Orobraze 950. It exhibits excellent high temperature strength up to 500°C and shows good resistance to oxidation at elevated temperatures. Orobraze 990 also offers good corrosion resistance in many chemical environments. This alloy has been used in the manufacture of aero-engine components for its high temperature properties.

Orobraze 990 is suitable for brazing in a vacuum because it contains no volatile elements. Grade 1 Orobraze 990 has impurity levels which make it suitable for brazing components that operate in an ultra high vacuum, such as vacuum tube devices. It is suitable for step brazing in complex assemblies.

Orobraze 990 differs from Orobraze 950 in that it has a 40°C melting range and consequently typical joint gaps are 0.075-0.2mm depending on parent metals and joint configuration.

Typical applications are for brazing stainless steel, high temperature nickel alloys and super alloys. It can be used for joining copper to these alloys in thermionic valve devices.

Orobraze 990 is most often used for brazing in reducing atmosphere or vacuum and under these conditions no flux is used. It can also be used in air with flame or induction heating if a suitable flux is employed.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 950 - 990 °C
Solidus 950 °C
Liquidus 990 °C
 
Component Elements PropertiesOriginal ValueComments
Gold, Au 75 %
Nickel, Ni 25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Johnson Matthey Orobraze™ 940 Gold-Copper Brazing Filler Metal
Johnson Matthey Orobraze™ 910 Gold-Copper Brazing Filler Metal
Johnson Matthey Orobraze™ 970 Gold-Copper Brazing Filler Metal
Johnson Matthey Orobraze™ 950 Gold Bearing Brazing Filler Metal
Henkel Loctite® 3880 Heat Cure Isotropic Epoxy Adhesive

NJMMJ9745 / 186146

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.