MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset

Material Notes: Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.

Key features and benefits are:

  • Good dimensional stability, including excellent thermal resistance
  • Pigmentable for molded-in color; best appearance with mold texture
  • Excellent property retention in cold and hot environments
  • Suitable for outdoor use in applications involving UV exposure and water immersion in accordance with UL746C (f1), see file E42524
  • Designed for compression molding in matched metal die molds.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 - 1.85 g/cc
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cmPolymerization Shrinkage
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 75.0 MPaASTM D638
Tensile Modulus 12.0 GPaASTM D638
Flexural Strength 180 MPaASTM D790
Flexural Modulus 11.0 GPaASTM D790
Compressive Strength 215 MPaASTM D695
Poissons Ratio 0.30
Shear Modulus 4.60 GPaCalculated
Izod Impact, Notched 800 J/mASTM D256
Izod Impact, Unnotched 11.5 J/cmASTM D4812
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 15.0 kV/mmASTM D149
Arc Resistance 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°CZ Direction
CTE, linear, Transverse to Flow 25.0 µm/m-°CXY Direction
Thermal Conductivity 0.300 W/m-K
UL RTI, Electrical 130 °CUL 746C
UL RTI, Mechanical with Impact 130 °CUL 746C
UL RTI, Mechanical without Impact 130 °CUL 746C
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 °CCompression Molding
Clamp Pressure 500 - 1000 psiMolding Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC
A. Schulman Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC
A. Schulman Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC
C-Glass Fiber, Generic
A. Schulman Premi-Glas® 1200-30 Polyester SMC

PPREMH956 / 140354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.