MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® U 2500 TEM Two-Component Polyurethane Encapsulant
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Loctite Stycast U 2500 TEM provides the following product characteristics:
  • Low viscosity
  • Flexible
  • Excellent wetting properties

Cure: Room Temperature or Heat Cure

Application: Encapsulant

Typical Assembly Applications: Transformers, PCB's and other insulating applications

Loctite Stycast U 2500 TEM flexible polyurethane encapsulant is formulated to have low viscosity and excellent wetting properties allowing complete impregnation of either small slightly wound coils or large castings.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccPart B
 1.50 g/ccPart A
Moisture Absorption 0.800 %
@Time 86400 sec
Viscosity 5.0 cPPart B
 6000 cPMixed
 12500 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
Tensile Strength 3.50 MPa
Elongation at Break 70 %
Modulus of Elasticity 0.00700 GPa
Adhesive Bond Strength 2.50 MPaTensile Lap Shear Strength, Al to Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+11 ohm-cm500 Volts
Surface Resistance 1.00e+14 ohm
Dielectric Constant 6.0
@Frequency 1e+6 Hz
Dissipation Factor 0.060
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 175 µm/m-°C
Thermal Conductivity 0.600 W/m-K
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg -68.0 °CTMA
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 60.0 °C
Alternate, A post cure of 2 hours @ 100 to 120°C is recommended.
 24.0 hour
@Temperature 25.0 °C
Recommended, Post cure of 2 hours @ 100 to 120°C is recommended.
Pot Life 45.0 min
Shelf Life 6.00 Month
@Temperature 18.0 - 25.0 °C
 
Descriptive Properties
AppearanceAmberPart B
 BlackPart A
Mix Ratio, by Volume100 : 8.5Part A : Part B
Mix Ratio, by Weight100 : 7Part A : Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7963 / 255447

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.