MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Axiall 8268 Rigid PVC, Extrusion  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf 8268 is a rigid PVC pellet compound suited for applications where transparency is important. It is widely used for clear profiles such as furniture trim, shower door and protected jalousie windows. High impact vacuum formed sheet applications are also filled with 8268. Twin screw machines may be used to convert Georgia Gulf 8268. 8268 is characterized by excellent physical properties and easy processing. It contains UV inhibitor to retard deterioration. It is available in fiberboard boxes, railroad bulk hopper cars or bulk truckloads.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 112112ASTM D-785
Hardness, Shore D 7979ASTM D-2240
Tensile Strength, Yield 44.8 MPa6500 psiASTM D-638
Tensile Modulus 2.62 GPa380 ksiASTM D-638
Flexural Strength 81.4 MPa11800 psiASTM D-790
Flexural Modulus 2.62 GPa380 ksiASTM D-790
Izod Impact, Notched 6.41 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
12.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 187 kJ/m²89.0 ft-lb/in²ASTM D-1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C162 °FASTM D-648
Flammability, UL94 V-0V-0
 
Descriptive Properties
Cell Classification14444333ASTM D-4216

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Douglas-fir Plywood

PGGUL422 / 41698

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.