MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Magnesium ZE63A-T6, Cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Nd content refers to Nd-rich rare earths. Aerospace and military sand and investment castings used in solution heat treated and artificially aged condition (T6 temper). Has excellent castability and pressure tightness. Especially useful in thin-section castings for applications requiring high mechanical strength and freedom from porosity. Special heat treatment in hydrogen is required to develop mechanical properties, which results in a wall thickness limitation for the castings.

Key Words: UNS M16630; Mg; ASTM B 93 (Ingot UNS M16631)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.87 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 60 - 85500 kg load, 10 mm ball
Hardness, Knoop 93Estimated from Brinell
Hardness, Vickers 80Estimated from Brinell
Tensile Strength, Ultimate 300 MPa
Tensile Strength, Yield 190 MPa
@Strain 0.2 %
Elongation at Break 10 %in 50 mm
Tensile Modulus 45.0 GPa
Compressive Yield Strength 195 MPaat 0.2% offset
Compressive Strength 65000 psi
Compressive Modulus 44.0 GPa
Poissons Ratio 0.35
Fracture Toughness 27.0 MPa-m½Plane-Strain
Machinability 100 %Relative Rating, 100=Best
Shear Modulus 17.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000560 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 370 J/gEstimated from trends in similar Mg alloys.
CTE, linear 26.5 µm/m-°C
@Temperature 0.000 - 100 °C
 27.1 µm/m-°C
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.960 J/g-°C
Thermal Conductivity 109 W/m-K
Melting Point 510 - 635 °C
Solidus 510 °C
Liquidus 635 °C
 
Processing PropertiesOriginal ValueComments
Casting Temperature 750 - 820 °CSand Casting
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu <= 0.10 %
Magnesium, Mg 91 %
Neodymium, Nd 2.1 - 3.0 %
Nickel, Ni <= 0.010 %
Zinc, Zn 5.5 - 6.0 %
Zirconium, Zr 0.40 - 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium ZE41A-T5, Cast
Magnesium EA55RS-T4, Extruded
Magnesium EA65RS-T4, Extruded
Magnesium Elektron Elektron® 675 Magnesium Wrought Alloy
Magnesium Elektron Elektron® ZK60A Magnesium Alloy, UNS M16600

MMZE63 / 12473

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.