MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hyosung Topilene HB240P PP
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: Topilene® HB240P is a specially designed polypropylene block copolymer (PP-B, natural colored) that features excellent long-term hydrostatic pressure resistance. It is suitable for underground drainage & sewage pipes and fittings. It is the outcome of HYOSUNG's integrated polymerization and crystallization technology with advanced PP manufacturing process technique.

Typical Applications: Drainage & sewage pipes and fittings (Solid wall &twin wall corrugated pipes system)/ Industrial pipes

Features: Excellent long-term hydrostatic pressure resistance/ Excellent stiffness and impact strength balance / Enhanced big diameter pipe manufacturing processability / Chemical stability / Environment-friendly

Compliance: The pipes produced with Topilene®HB240Pcomplies with the hydrostatic pressure requirements according to ISO/DIS 15874.It complies with the requirements of FDA21 CFR 177.1520. This product corresponds to GB/T17219-1998 for drinking water system.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 0.35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.35 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Storage Temperature 40.0 °C104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8585ASTM D785
Tensile Strength, Yield 31.4 MPa4550 psiASTM D638
Flexural Modulus 1.47 GPa213 ksiASTM D790
Izod Impact, Unnotched NBNBASTM D256
 0.490 J/cm
@Temperature -10.0 °C
0.918 ft-lb/in
@Temperature 14.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 155 °C311 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 30.0 °C68.0 - 86.0 °FCooling Temperature
 200 - 235 °C392 - 455 °FMixing Zone
Feed Temperature 170 - 190 °C338 - 374 °F
Die Temperature 200 - 235 °C392 - 455 °F
Melt Temperature 190 - 225 °C374 - 437 °FMelting Zone
 200 - 235 °C392 - 455 °F
Head Temperature 200 - 235 °C392 - 455 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourair circulated condition

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hyosung Topilene J340 PP
Hyosung Topilene HJ340 PP
Hyosung Topilene B240T PP
Braskem INSPIRE™ 114 Performance Polypropylene Polymer
Avient Maxxam™ FR PP 301 EXT Polypropylene

PHYOS52 / 47938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.