MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibility

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 40000 - 90000 cPBase
 40000 - 90000 cPAccelerator
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 45
Elongation at Break 40 %
Shear Strength 40.0 - 60.0 psiOverlap, Neoprene Rubber/Steel
 80.0 - 100 psiOverlap, SBR/Steel
 150 psiOverlap, Abraded Aluminum, 14 days in 5% salt spray @ 35°C
 390 psiOverlap, PVC/PVC, Rigid
 480 psiOverlap, Acrylic/Acrylic
 500 psiOverlap, Etched Aluminum, 14 days in 5% salt spray @ 35°C
 680 psiOverlap, ABS/ABS Plastic
 680 psiOverlap. PC/PC
 700 psiOverlap, Abraded Aluminum, 3 days, 71°C, 100% RH
 1200 psiOverlap, Etched Aluminum, 3 days, 71°C, 100% RH
 1250 psiOverlap, Abraded Aluminum, 30 days tap water @ RT
 1400 psiOverlap, Fiber Reinforced Polyester/Fiber Reinforced Polyester
 1750 psiOverlap, Copper/Copper
 2300 psiOverlap, Al/Al
 2300 psiOverlap, Etched Aluminum, 30 days tap water @ RT
 2300 psiOverlap, Abraded Aluminum, Initial
 2450 psiOverlap, Stainless Steel/Stainless Steel
 2450 psiOverlap, Brass/Brash
 2500 psiOverlap, CRS/CRS
 2500 psiOverlap, Etched Aluminum, Initial
 2600 psiOverlap, Galvanized Steel/Galvanized Steel
 250 psi
@Temperature 82.0 °C
Overlap
 270 psi
@Temperature 71.0 °C
Overlap
 2700 psi
@Temperature -55.0 °C
Overlap
 3500 psi
@Temperature 24.0 °C
Overlap
Peel Strength 20.0 pliT-Peel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.90e+10 ohm-cm
Dielectric Strength 470 kV/in
 
Thermal PropertiesOriginal ValueComments
CTE, linear 73.0 µm/m-°C
@Temperature -50.0 - 0.000 °C
 165 µm/m-°C
@Temperature -50.0 - 110 °C
Thermal Conductivity 1.25 BTU-in/hr-ft²-°F
@Temperature 45.0 °C
Glass Transition Temp, Tg 16.0 °C
 
Descriptive Properties
AppearanceBlack
 GrayBase
 WhiteAccelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive

PMM34620 / 169367

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.