MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC LNP™ STAT-KON™ RFD02 PA 66 (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP STAT-KON RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.

Information provided by SABIC Innovative Plastics for Asia Pacific.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ASTM D 792
 1.30 g/cc0.0470 lb/in³ISO 1183
Moisture Absorption 0.500 %
@Time 86400 sec
0.500 %
@Time 24.0 hour
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow  0.010 - 0.012 cm/cm
@Time 86400 sec
0.010 - 0.012 in/in
@Time 24.0 hour
ASTM D 955
 0.011 cm/cm
@Time 86400 sec
0.011 in/in
@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse  0.015 cm/cm
@Time 86400 sec
0.015 in/in
@Time 24.0 hour
ISO 294
 0.014 - 0.016 cm/cm
@Time 86400 sec
0.014 - 0.016 in/in
@Time 24.0 hour
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 74.0 MPa10700 psiISO 527
 77.0 MPa11200 psiASTM D 638
Elongation at Break 5.1 %5.1 %ISO 527
 5.5 %5.5 %ASTM D 638
Tensile Modulus 7.40 GPa1070 ksi1 mm/min; ISO 527
 8.27 GPa1200 ksi50 mm/min; ASTM D 638
Flexural Strength 131 MPa19000 psiASTM D 790
 139 MPa20200 psiISO 178
Flexural Modulus 5.51 GPa799 ksiASTM D 790
 6.30 GPa914 ksiISO 178
Izod Impact, Notched 0.370 J/cm
@Temperature 23.0 °C
0.693 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 2.13 J/cm
@Temperature 23.0 °C
3.99 ft-lb/in
@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 3.00 kJ/m²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 14.0 kJ/m²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
80*10*4; ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 ohm - 1e+05100 ohm - 1e+05ASTM D 257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  68.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E 831
 69.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  46.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
26.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E 831
 48.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
26.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 256 °C493 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 252 °C
@Thickness 3.20 mm
486 °F
@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 239 °C462 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 236 °C
@Thickness 3.20 mm
457 °F
@Thickness 0.126 in
unannealed; ASTM D 648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber

PSABI48186 / 189271

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.