MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ELM® NSF H1 Food Grade Chain and Cable Lubricant
Categories: Fluid; Lubricant

Material Notes: Description: ELM Chain Lubricant – Food Grade is a high performance food grade chain lubricant formulated with the best optimized USA-grown natural seed oils and select additives, it surpasses the lubricity and performance of conventional chain lubricants. It is NSF (National Sanitary Foundation) approved H1 for incidental food contact. NSF Registration No. 142552

Applications:

  • General purpose chain lubricant
  • Use for chains, cables, rollers
  • NSF H1 Approved for incidental food contact
Benefits:
  • Reduces product inventory
  • Superior lubricity improves productivity
  • Less mist generation
  • Safe for all metals
  • Will help your business comply with ISO-14000
  • Does not contain chlorine
  • High flash and fire points
  • Made from renewable USA-grown crop-based vegetable oils

Information provided by ELM®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Kinematic Viscosity at 40°C (104°F) 44 cSt44 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Flash Point 306 °C583 °FASTM D92
 
Descriptive Properties
AppearanceLight Yellow
Fire Point324°CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Sealing Solutions Turcite® TA Self-Lubricating Thermoplastic Rod
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
Nye Lubricants 179A (SO) Synthetic Oil
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer
Ensinger Tecamid® GF30 Extruded Nylon 6/6 30% glass-fiber-reinforced (PA66)

WELML021 / 146224

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.