MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hifax™ RTA3263/2 Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hifax™ RTA3263/2 medium melt flow, 1,700 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of rigidity, impact strength and paintability. It was designed primarily for rigid automotive exterior ornamentation applications. Uses: Automotive exterior parts

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183 & ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm0.0070 in/in0.125 in; ASTM D955
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767ISO 868 & ASTM D2240
Tensile Strength at Break 17.2 MPa2500 psiASTM D638
Tensile Strength, Yield 20.0 MPa2900 psiISO 527-1, -2
 20.7 MPa3000 psiASTM D638
Elongation at Break 300 %300 %ASTM D638
Elongation at Yield 10 %10 %ISO 527-1, -2 & ASTM D638
Flexural Modulus 1.70 GPa247 ksiISO 178
 1.72 GPa250 ksiASTM D790
Izod Impact, Notched (ISO)  3.30 kJ/m²
@Temperature -40.0 °C
1.57 ft-lb/in²
@Temperature -40.0 °F
ISO 180
 5.90 kJ/m²
@Temperature -30.0 °C
2.81 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 21.0 kJ/m²
@Temperature 23.0 °C
9.99 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Gardner Impact 14.0 J
@Temperature -30.0 °C
10.3 ft-lb
@Temperature -22.0 °F
ASTM D3029, tested in accordance with ASTM D5420
Dart Drop, Total Energy 17.0 J
@Temperature -30.0 °C
12.5 ft-lb
@Temperature -22.0 °F
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763
Tear Strength 105 kN/m600 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FUnannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 56.1 °C133 °FUnannealed; ISO 75A-1, -2
Shrinkage 0.70 %0.70 %Tool, 100x150x3.2 mm; Basell Test Method
 0.90 %
@Temperature 121 °C,
Time 3600 sec
0.90 %
@Temperature 250 °F,
Time 1.00 hour
Afterbake, 100x150x3.2 mm; Basell Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMO800 / 53789

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.