MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ixef® 1028 Polyarylamide (PARA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyarylamide (PAA); Polyarylamide, Glass Fiber Filled

Material Notes: Ixef 1028 is a laser printable, 50% glass-fiber reinforced polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1028/9208

Injection Notes: Hot Runner: 250°C to 260°C (482°F to 500°F) Drying The material as supplied is ready for molding without drying. However, If the bags have been open for longer than 24 hours, the material needs to be dried. When using a desiccant air dryer with dew point of -28°C (-18°F) or lower, these guidelines can be followed: 0.5-1.5 hour at 120°C (248°F), 1-3 hours at 100°C (212°F), or 1-7 hours at 80°C (176°F). Injection Molding IXEF 1028 compound can be readily injection molded in most screw injection molding machines. A general purpose screw is recommended, with minimum back pressure. The measured melt temperature should be about 280°C (536°F), and the barrel temperatures should be around 250°C to 260°C (482°F to 500°F) in the rear zone, gradually increasing to 260°C to 290°C (500°F to 554°F) in the front zone. If hot runners are used, they should be set to 250°C to 260°C (482 to 500°F). To maximize crystallinity, the temperature of the mold cavity surface must be held between 120°C and 140°C (248°F and 284°F). Molding at lower temperatures will produce articles that may warp, have poor surface appearance, and have a greater tendency to creep. Set injection pressure to give rapid injection. Adjust holding pressure and hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled (95%-99%).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Filler Content 50 %Unspecified Filler
Water Absorption 0.17 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 1.6 %65% RH
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 250 MPaISO 527-2
Elongation at Break 1.8 %ISO 527-2
Tensile Modulus 20000 MPaISO 527-2
Flexural Strength 360 MPaISO 178
Flexural Modulus 18500 MPaISO 178
Izod Impact, Notched 80.0 J/mASTM D256
Izod Impact, Unnotched 7.30 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 17.0 µm/m-°CISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 225 °CUnannealed; ISO 75-2/A
Flammability, UL94 HBUL 94
Oxygen Index 26 %ISO 4589-2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 260 °C
Front Barrel Temperature 260 - 290 °C
Melt Temperature 280 °C
Mold Temperature 120 - 140 °C
Drying Temperature 120 °C
@Time 1800 - 5400 sec
 
Descriptive Properties
AppearanceBlack
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
FeaturesGood Chemical Resistance
 Good Creep Resistance
 Good Dimensional Stability
 High Flow
 High Strength
 Laser Markable
 Low Moisture Absorption
 Outstanding Surface Finish
 Ultra High Stiffness
FormsPellets
Injection RateFast
Processing MethodInjection Molding
RoHS ComplianceRoHS Compliant
UsesAppliance Components
 Appliances
 Automotive Electronics
 Business Equipment
 Cams
 Electrical Housing
 Electrical/Electronic Applications
 Furniture
 Gears
 Industrial Applications
 Lawn and Garden Equipment
 Machine/Mechanical Parts
 Metal Replacement
 Power/Other Tools

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Ixef® 1023 Polyarylamide (PARA)
Syensqo (Solvay Specialty Polymers) Ixef® 2060 Polyarylamide (PARA)
Lehvoss LUVOCOM® 16/XCF/25 Polyarylamide with carbon fiber
Overview of materials for Polyarylamide, Glass Fiber Filled
RTP Company RTP 285 K TFE 15 Polyarylamide (PAA), Carbon Fiber - PTFE Lubricated

PSOL8Y887 / 107671

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.