MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exxtral™ HMU 404 Performance Polyolefin
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: A specialty thermoplastic polyolefin resin, black colored, characterized by very high stiffness and high heat stabilization. Typically used in automotive heating and air conditioning units.

Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America

Features:

  • Good Dimensional Stability
  • Ultra High Stiffness
Uses:
  • Automotive Applications
  • Automotive Interior Parts
  • Automotive Under the Hood
  • Consume Applications
Processing Method: Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 4500 psiISO 527-2/50
Tensile Strength, Yield 4790 psiISO 527-2/50
Elongation at Break 4.5 %ISO 527-2/50
Elongation at Yield 3.1 %ISO 527-2/50
Tensile Modulus 580000 psiSecant; ISO 527-2
Charpy Impact, Notched 1.30 ft-lb/in²
@Temperature 22.8 °C
Complete Break; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 259 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 158 °FISO 75-2/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Exxtral™ HMU 405 Performance Polyolefin
Alcoa KAMA 7110 Clear Homopolymer Polypropylene (PP)
Arkema Kynar® 710 Polyvinylidene Fluoride Homopolymer- Injection Molding
RTP Company RTP 3382 Polyvinylidene Fluoride (PVDF), Carbon Fiber
ExxonMobil Exxtral™ CMW 402 Performance Polyolefin

PEX99381 / 175617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.