MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay ABEX® EP 110 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Proprietary surfactant system for emulsion polymerization

Identification: ETHOXYLATED NONYLPHENOL SULPHATE AMMONIUM SALT WATER SOLUTION

CAS: 68649 – 55 – 8; 7732-18-5

Solubility: Soluble in water. Insoluble in polar and aromatic solvents.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Emulsifier for polymerization in emulsion of Vinyl acetate homopolymer, Vinyl acetate/acrylates, Acrylics, Styrene/acrylic, Styrene/butadiene

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
pH 6.5 - 7.510% in water; RPG02
Surface Tension 37 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Fe (Iron) <= 5.0 ppmRPG27
 
Thermal PropertiesOriginal ValueComments
Pour Point <= 0.000 °C
Flash Point >= 100 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 3.0RPG18
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear, clean liquidRPG31
CompositionActive content0.31
 Ammonium Sulfate<1%, RPG77
 Anionic active substance28-31%, RPG 12
 Dry substance30-33%, RPG25
 KATHON as 100% active5-15 ppm, RPG107
 Nonionic<2%, RPG35
Critical Micelle Concentration (%)0.1
Ionic ChargeAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODAPEX® CO-436 Surfactant
Solvay ABEX® EP 120 Surfactant

WRHOD002 / 137232

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.