MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arla SAPHIR® PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: SAPHIR® is hard coated polycarbonate sheet with glass like appearance suitable for flat applications. The high impact strength of polycarbonate is combined with improved weather and chemical resistance. The product offers protection against abrasion compared to standard plastic sheets. SAPHIR® is resistant to many of the most common chemicals, and the hard coat also provides an excellent protection against graffiti and vandalism. SAPHIR® weighs about half of standard glass, yet the product is virtually unbreakable. SAPHIR® has an outstanding clarity, the hard coat improves the light transmission of the polycarbonate sheet.

Benefits: Abrasion and Impact Resistant; Chemical Resistance; UV Stability; High optical quality and outstanding clarity; More than 10 times the impact strength of high impact PMMA

Application: Anti-vandal glazing, security glazing, safety screens and acoustic screens, Industrial equipment (machine coverings, machine protections), Indoor and outdoor signs, vending machine faces and many different kinds of technical parts.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Moisture Absorption 0.150 %
@Time 86400 sec
50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaISO 527
Tensile Strength, Yield 60.0 MPaISO 527
Elongation at Break 110 %ISO 527
Elongation at Yield 6.0 %ISO 527
Modulus of Elasticity >= 2.30 GPaISO 527
Flexural Modulus >= 2300 MPaISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 65.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -40.0 °C
ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
Abrasion 2.0
@Load 0.500 kg
% Haze; Taber, CS 10F, 500 cycles; ASTM D1044
 <= 9.0
@Load 0.500 kg
% Haze; Taber, CS 10F, 500 cycles; ASTM D1044
 
Thermal PropertiesOriginal ValueComments
CTE, linear 65.0 µm/m-°C
@Temperature 20.0 - 70.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KDIN 8302
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ISO 489

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARLA939 / 301117

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.